Metal Hardness Converter (HRC, HBW, HV) | Muhendis Portal

Convert Rockwell C (HRC), Brinell (HBW), Vickers (HV), Rockwell B (HRB) and approximate tensile strength (MPa) per ISO 18265 and ASTM E140.

Verified Engineering Calculation Engine

Engineered for mechanical, HVAC, piping, and design engineers in compliance with international standards (ISO, DIN, EN, ASME, ASHRAE). Load the interactive tool for real-time calculations and automated reports.

ISO 18265 / ASTM E140 Steel Hardness Conversion Reference Table

Standard conversion chart across Rockwell C (HRC), Brinell (HBW), Vickers (HV), and approximate tensile strength (MPa).

Rockwell C (HRC)Brinell (HBW 10/3000)Vickers (HV)Tensile Strength Rm (MPa)
20 HRC226 HBW238 HV770 MPa
28 HRC271 HBW286 HV930 MPa
32 HRC301 HBW318 HV1,015 MPa
38 HRC353 HBW372 HV1,180 MPa
42 HRC390 HBW412 HV1,320 MPa
48 HRC455 HBW484 HV1,560 MPa
54 HRC543 HBW577 HV1,920 MPa
60 HRC654 HBW697 HV— (>2,150 MPa)

Frequently Asked Questions (FAQ)

How much is 60 HRC in Brinell (HBW) and Vickers (HV)?

Per ISO 18265 conversion tables for carbon and low-alloy steels, 60 HRC corresponds to approximately 654 HBW and 697 HV.

Related Technical Guides